Requirements vary by sealing design and governing specification. Do not assume that all oil and gas sealing surfaces require sub-micron Ra. Use the applicable component drawing and standard. For example, ASME B16.5 specifies a maximum 1.6 μm (63 μin.) roughness for ring-joint groove side walls and 3.2–6.3 μm (125–250 μin.) average roughness for other specified flange facings.
API 6A is a specification for wellhead and tree equipment. It includes requirements covering areas such as design, materials, inspection and testing. Grinding can help achieve specified geometry and surface characteristics, but grinding alone does not establish API 6A compliance.
Cylindrical grinding can provide controlled diameter, cylindricity, concentricity and surface finish for shafts, sleeves, bearing surfaces, seal areas and selected bores where those characteristics are required.
Nickel-based alloys such as Inconel 625 and 718, duplex and super duplex stainless steels, and titanium can require carefully controlled grinding processes. Wheel selection, dressing, cutting parameters, coolant delivery and machine rigidity should be matched to the material and application.
Start with the component drawing and process requirements: workpiece size, material, grinding type, dimensional tolerances, surface finish, production volume and inspection method. Then select a machine configuration whose published capability and application support match those requirements.